www.人妻系列,国产AV在线观看吧,国内大学美女自拍视频,亚洲日韩无线免费观看

Welcome to the Jinzhou Swan Welding Consumables Co.,Ltd official website   中文版 ENGLISH
  Product category
    Welding rod
   Low-alloy and high strength steel electrode
   Low-alloy heat-resistance steel electrode
   Cr-Ni stainless steel electrode1
   Surfacing electrode
   Cost iron electrode
   Cr-Ni stainless steel electrode
   Cost iron electrode1
   Low temperature steel electrode
    Welding flux
   JH-SJ101 Agglomerated fluxes
   JH-SJ101G Agglomerated fluxes
   JH-SJ101Q Agglomerated fluxes
   JH-SJ102 Agglomerated fluxes
   JH-SJ105 Agglomerated fluxes
   JH-SJ402 Agglomerated fluxes
   JH-SJ301 Agglomerated fluxes
   JH-SJ403 Agglomerated fluxes for overlaying
   JH-SJ501 Agglomerated fluxes
   JH-SJ501M Agglomerated fluxes
   JH-SJ503 Agglomerated fluxes
   JH-SJ601 Agglomerated fluxes
   JH-SJ181q Agglomerated fluxes
    Welding Wire
   JH-H08A Submerged arc welding wires
   JH-H08MnA Submerged arc welding wires
   JH-H10Mn2 Submerged arc welding wires
   JH-H08E Submerged arc welding wires
   JH-WQ1 Submerged arc welding wires
   Jh-WQ3 Submerged arc welding wires
   JH-WQ4 Submerged arc welding wires
   JH-WWGX2 Submerged arc welding wires
  Products Home>Products
 

【JH-Sj402 Agglomerated fluxes】
 


  Explanation:JH-SJ402 is a soda-fluorine type agglomerated flux, alkalinity around 0.7. It is gray and round grain, with grain size around 2.0~0.28mm.It can be operated with AC and DC,the wire shall be perfect deposit metal mechanical properties.
  Applications:With suitable wire of H08A, to be mainly applied in the welding of low carbon steel and some low alloy steel structures,and the submerged weking of locomotive wagon,mining equipments, It’s suitable in the welding of thin steel plates and medium thickness steel plates, especially for the high speed welding of thin plates.The deposit metal has perfect mechanical properties.

  Chemical Composition of Flux

  Mechanical Properties of Deposit Metal

  Points of Attention:
  1 The  fluxs  to be dried 2 hours in 300℃~350℃.
  2 De-rusting, water and oil cleaning ,as well other impurities removing of the work be done before welding.

 